Structure and mechanical properties of porous TiNi alloys with Ag nanoparticles

The work studies the influence of the silver dopant (<0.5 at.%) on the structure and mechanical properties of porous TiNi alloys obtained by self-propagating high-temperature synthesis. These alloys are of high scientific and practical interest in medicine. The presence of silver in the TiNi allo...

Full description

Bibliographic Details
Published in:Coatings Vol. 13, № 1. P. 24 (1-13)
Other Authors: Marchenko, Ekaterina S., Baigonakova, Gulsharat A., Larikov, Viktor, Monogenov, Alexander N., Yasenchuk, Yuriy F.
Format: Article
Language:English
Subjects:
Online Access:http://vital.lib.tsu.ru/vital/access/manager/Repository/koha:001009173
Перейти в каталог НБ ТГУ
LEADER 02915nab a2200385 c 4500
001 koha001009173
005 20231113114959.0
007 cr |
008 231103|2022 sz s a eng d
024 7 |a 10.3390/coatings13010024  |2 doi 
035 |a koha001009173 
040 |a RU-ToGU  |b rus  |c RU-ToGU 
245 1 0 |a Structure and mechanical properties of porous TiNi alloys with Ag nanoparticles  |c E. S. Marchenko, G. A. Baigonakova, V. Larikov [et al.] 
336 |a Текст 
337 |a электронный 
504 |a Библиогр.: 29 назв. 
520 3 |a The work studies the influence of the silver dopant (<0.5 at.%) on the structure and mechanical properties of porous TiNi alloys obtained by self-propagating high-temperature synthesis. These alloys are of high scientific and practical interest in medicine. The presence of silver in the TiNi alloy will ensure improved cytocompatibility and antibacterial properties. The TiNi porous alloys with 0.2 and 0.5 at.% Ag nanoparticles have multiphase composition. Quantitative X-ray diffraction analysis of the obtained alloys showed that an increase in the silver content is accompanied by a quantitative decrease in the austenite phase TiNi(B2) and an increase in the martensite phase TiNi(B19'), as well as in secondary phases Ti2Ni, Ti4Ni2O. Evenly distributed silver nanoparticles up to 10 nm were found in the surface layer by transmission electron microscopy. The results of the scanning electron microscopy showed that inclusions containing silver are located mainly in the zones of Ti2Ni peritectic crystallization. The mechanical characteristics were studied by means of compression tests and it was found that with an increase in the silver dopant, the elastic modulus and elastic limit decrease, but the maximum deformation to fracture increases significantly. It was found that with an increase in the volume fraction of silver, the plastic properties of the alloy increase. No dependency of the tensile strength on the amount of silver was found. 
653 |a механические характеристики 
653 |a наночастицы 
653 |a пористые сплавы 
653 |a серебро 
653 |a сплавы TiNi 
655 4 |a статьи в журналах  |9 898502 
700 1 |a Marchenko, Ekaterina S.  |9 275843 
700 1 |a Baigonakova, Gulsharat A.  |9 275840 
700 1 |a Larikov, Viktor  |9 898503 
700 1 |a Monogenov, Alexander N.  |9 856919 
700 1 |a Yasenchuk, Yuriy F.  |9 275839 
773 0 |t Coatings  |d 2022  |g Vol. 13, № 1. P. 24 (1-13)  |x 2079-6412 
852 4 |a RU-ToGU 
856 4 |u http://vital.lib.tsu.ru/vital/access/manager/Repository/koha:001009173 
856 |y Перейти в каталог НБ ТГУ  |u https://koha.lib.tsu.ru/cgi-bin/koha/opac-detail.pl?biblionumber=1009173 
908 |a статья 
999 |c 1009173  |d 1009173 
039 |b 100