In situ characterization of the functional degradation of a [001] orientated Fe-Mn-Al-Ni single crystal under compression using acoustic emission measurements

Acoustic emission (AE) measurements were conducted in situ during cyclic compressive loading on an [ 00 1 over line ] orientated single crystal of Fe-Mn-Al-Ni shape memory alloy to study functional degradation of its superelastic response. The acoustic investigations were corroborated by optical mic...

Full description

Bibliographic Details
Published in:Acta materialia Vol. 220. P. 17333 (1-19)
Other Authors: Weidner, Anja, Vinogradov, Alexei, Vollmer, Malte, Krooß, Philipp, Kriegel, Mario J., Klemm, Volker, Chumlyakov, Yuri I., Niendorf, Thomas, Biermann, Horst