Effect of ultrasonic melt treatment on the refinement of primary Al3Ti intermetallic in an Al-0.4Ti alloy

High intensity ultrasonic melt treatment was applied to an Al-0.4 wt% Ti alloy over three selected temperature ranges: 810 to 770 °C (above liquidus), 770 to 730 °C (across liquidus), and 730 to 690 °C (below liquidus). The size and morphology of the primary Al3Ti intermetallic particles were studie...

Full description

Bibliographic Details
Published in:Journal of crystal growth Vol. 435. P. 24-30
Other Authors: Wang, Feng, Connolley, Thomas, Mi, Jiawei, Eskin, Dmitry G.