Microstructure and hot deformation behavior of the Cu-1Ni-0.9Sn-0.5Ti-0.3Cr alloy

The Cu-1Ni-0.9Sn-0.5Ti-0.3Cr alloy was prepared by vacuum induction melting. The hot deformation experiments with the alloy were carried out using the Gleeble-1500 deformation simulation device at 0.001-10 s−1 strain rate, and 500-900 °C deformation temperature. The hot working constitutive equation...

Full description

Bibliographic Details
Published in:Materials today communications Vol. 31. P. 103771 (1-13)
Other Authors: Tang, Shunlong, Zhou, Meng, Li, Xu, Zhang, Yi, Xu, Deye, Zhang, Zhiyang, Tian, Baohong, Jia, Yanlin, Liu, Yong, Volinsky, Alex A., Marchenko, Ekaterina S.